As welded | ||
Elongation | Tensile Strength | Yield Strength |
36 % | 570 MPa | 400 MPa |
Tested at 350°C. As welded | ||
Elongation | Tensile Strength | Yield Strength |
25 % | 490 MPa | 370 MPa |
As welded | |
Impact Value | Testing Temperature |
110 J | 20 °C |
70 J | -60 °C |
45 J | -196 °C |
Mn | |||||||
Mn | Mo | Cu | C | Si | Ferrite FN | Ni | Cr |
1.8 % | - | - | - | - | - | - | - |
Mo | |||||||
Mn | Mo | Cu | C | Si | Ferrite FN | Ni | Cr |
- | 0.15 % | - | - | - | - | - | - |
Cu | |||||||
Mn | Mo | Cu | C | Si | Ferrite FN | Ni | Cr |
- | - | 0.10 % | - | - | - | - | - |
C | |||||||
Mn | Mo | Cu | C | Si | Ferrite FN | Ni | Cr |
- | - | - | 0.01 % | - | - | - | - |
Si | |||||||
Mn | Mo | Cu | C | Si | Ferrite FN | Ni | Cr |
- | - | - | - | 0.9 % | - | - | - |
Ferrite FN | |||||||
Mn | Mo | Cu | C | Si | Ferrite FN | Ni | Cr |
- | - | - | - | - | 9 % | - | - |
Ni | |||||||
Mn | Mo | Cu | C | Si | Ferrite FN | Ni | Cr |
- | - | - | - | - | - | 10.5 % | - |
Cr | |||||||
Mn | Mo | Cu | C | Si | Ferrite FN | Ni | Cr |
- | - | - | - | - | - | - | 19.9 % |
直径 | 安培 | 熔敷率 | 电压 V | 送丝速度 |
0.6 mm | - | - | - | - |
0.8 mm | 55-160 A | 1.0-4.1 kg/h | 15-24 V | 4.0-17.0 m/min |
0.9 mm | 65-220 A | 1.1-5.4 kg/h | 15-28 V | 3.5-18.0 m/min |
1.0 mm | 80-240 A | 1.5-6.0 kg/h | 15-28 V | 4.0-16.0 m/min |
1.14 mm | - | - | - | - |
1.2 mm | 100-300 A | 1.6-7.5 kg/h | 15-29 V | 3.0-14.0 m/min |
1.6 mm | 230-375 A | 5.2-8.6 kg/h | 23-29 V | 5.5-9.0 m/min |
品牌: | 瑞典伊萨焊材 |
型号: | OK AUTROD 308LSi |
加工定制: | 否 |
适用范围: | 焊接 |
用途: | 焊接 |
类型: | 不锈钢 |
规格: | 2.0-5.0 |